How to improve woolen and worsted mill operations (1900)
New York, N.Y. : McGraw-Hill · leaf 77
eed of the sizeroll. No doctor blade is used. After the carpet is sized, the pileis brushed and the carpet is steamedin a unit made bv H. W. Butterworth& Sons Co.. Inc. .\fter leaving thesteamer, the carpet is dried at approxi-niatelv 240° F. in an Andrews &Goodrich. Inc., dryer unit.… … ROLL with let-off controlled by broke bondsopplies proper tension to the carpet. Thespiral brush (arrow) removes lint and dirtfrom the carpet bock. LIFT ROLL, hydroulicolly operated, raises thecarpet (arrow) out of reach of the size roll.The meter (upper right) indicates the speedof the size roll.…
Woolen and worsted manufacture · Textile factories
Internet Archive · UMass Dartmouth, Claire T. Carney Library · Public Domain Mark 1.0. Free to use for anything.