ied (Fig. 2) these rust spots, although so thin, already exhibit signs of flaking off. On leaving a stratum of water on the surface of an iron plate for twelve hours, and then removing the water by- evaporation, a stronger development of rust will be found, which — towards the edges of the plate… … Fig. 25 (natural size). — Sheet of iron perforated by rust; the white patches are the holes, and the dark lines show the flakes of rust in the act of peeling off. is apparent on a more decided scale than in the previous experiment. By pouring water once over an iron plate so as to thoroughly cover…