Leonard, Anna B, Robineau, Adelaide Alsop, 1865?-1929 · Syracuse, N.Y. [etc.] : Keramic Studio Publishing Co · leaf 162
he water not at hand,wipe thoroughly with alcohol. It is best to use for thispurpose a piece of silk, as this does not give off bits of lintand fuzz as cotton goods do. It is necessary to havechina upon which you use lustre absolutely clean. It mustbe handled as little as possible for any moisture… … A MEDIAEVAL HUNT—PLATE DESIGN—MRS. J. UNGER. imperceptible at the time, they will cause countless littlewhite specks when the piece is fired. Another cause of spotted lustre is moisture in the kiln,which settles on the china when the firing gets under wayand causes bad spots. This may be done away…