Inside Out Library · Explore

Internal Stresses in Laminated Construction (1923)

NASA Technical Reports Server (NTRS) · leaf 9

An illustration from Internal Stresses in Laminated Construction, 1923, leaf 9
cent relative humidity. Glueroom, 90° F., with 65 per cent relative humidity. Storage room, No. 3, 80° F., with 30 per cent relative humidity. Storage room, No. 2, 80° F., with 60 per cent relative humidity. Storage room, No. 1, 80° F., with 90 per cent relative humidity. SPECIMENS. The test… … Plate 1.—Laminated test specimens for tension across the grain, showing steps in manufacture. The laminations for the glued-up and free (not glued) test specimens, shown in plate 1/ were matched end to end and taken as near each other as possible. Two sticks, A and B (about 40 inches in length),…

NASA Technical Reports Server (NTRS)

Internet Archive · NASA Technical Reports · Public domain (US government work). Free to use for anything.

More pictures from Internal Stresses in Laminated Construction

More like this