t.In this way, plate after plate, weighing from 25 to 50 lbs. each, is formed in intervals of hardly a minute.Only gray iron, from fusible materials, will chill in this way. The plates thus made are roasted, i. c,exposed for 10 or 12 hours to a red-heat, either in an appropriate oven or in an open…