(Pattern No. 98.) 132 lb. = 20 per cent. No. 22 bleached.264 lb. = 40 ,, mechanical wood (pine).66 lb. = 10 ,, sulphite wood.99 lb. = 15 ,, china clay.99 lb. = 15 „ No. 18 unboiled.2 lb. 3 oz. aluminium sulphate.1 oz. 6h dr. water blue 3 E.1 dr. 19 gr. magenta.Three-quarter-sized. DYED PATTERNS ON… … 363 lb. 33 1b. 66 1b.198 lb. (Pattern No. 99.) = 55 per cent. No. 7 bleached. = 5 ,, china clay. - 10 „ No. 18.= 30 „ No. 24.8f oz. ultramarine.£ oz. rhodarnine. y sized. The cotton rags used for mottling are treated in thesame manner as given for linen rags ; the cutting out ofthe seams is,…