ne works automatically full width without any assist¬ ance, and will dye three or four pieces or 100 to 120 metres sewn end to end. The machine is specially suitable for velvets, plushes, etc., and all goods having a tendency to crease or streak or to dye unlevel. 6. In hydraulic pressing, rubbed… … This last circumstance usually produces nasty creases even if it does not cause rubbing. In a cylinder press, rubbing places occur at the ends by entering the goods into the press carelessly. This is particularly the case in a link press, as the roller slides over the goods. We have also the…