overing the portion of the plate required. On an even andcomplete layer having beenobtained, take a wax-taper(fig./), and next proceedimmediately to smoke theground; the taper must bekept in motion, in orderthat the whole of theground may be evenlyblacked: if the flame ofthe taper is allowed to… … fig. e.