Cyclopedia of textile work : a general reference library on cotton, woolen and worsted yarn manufacture, weaving, designing, chemistry and dyeing, finishing, knitting, and allied subjects (1911)

American School (Lansing, Ill.) · Chicago : American school of correspondence · leaf 194

An illustration from Cyclopedia of textile work : a general reference library on cotton, woolen and worsted yarn manufacture, weaving, designing, chemistry and dyeing, finishing, knitting, and allied subjects, 1911, leaf 194
Salt.The temperature of the dye bath is raised to 120° F., the materialentered and worked ten to fifteen minutes at this temperature, and then 167 158 TEXTILE CHEMISTRY AND DYEING from one-half to three-quarters of an hour longer in the gradually coolingbath. It is then wrung evenly, and dried… … duced upon woolen or worsted cloth containing cotton by theproper application of acid dyestuffs. Thus, if worsted cloth con-taining a white cotton thread is dyed with certain acid blacks, thecotton thread will not even be stained, whereas the wool will bedyed l)]ack. By working this same dyed cloth…

Textile fabrics · Textile industry