ided into two classes: (i) Normal tests, or those made in either air or water maintained at MASONRY. 113 about 21° C. (70° F.), and (2) accelerated tests, or those made in air,steam or water at a temperature of 45° C. (115° F.) and upward. Thetest pieces should be allowed to remain 24 hours in… … Fig. 5.—Form of Clip. Normal Test. be made, upon a clean glass plate [about 10 cm. (3.94 in.) square], fromcement paste of normal consistency. 50. A pat is immersed in water maintained as near 21° C. (70° F.)as possible for 28 days, and observed at intervals. A similar pat ismaintained in air at…

Railroad engineering · Railroads

Internet Archive · Northeastern University Library · Public Domain Mark 1.0. Free to use for anything.

More pictures from Manual of recommended practice for railway engineering and maintenance of way

More like this