The principles and practice of textile printing (1912)
Knecht, Edmund, 1861-1925, Fothergill, James Best · London : Charles Griffin · leaf 549
, and III. in the cold, and make to 1 litre before use. Black P.S.is employed when a denser black is wanted; for most purposes, however, theweaker and cheaper Black P. is sufficiently dark. After padding, which is done in any of the ordinary types of paddingmachine, the goods are carefully dried,… … Grind the ingredients together in a mill before use. Print on black paddedcloth; steam 3-4 minutes in the rapid ager; pass through a i per cent.solution of bichromate of soda at 50°-60° C, wash well, soap, and dry. Zinc Oxide Discharges.—In these discharges, the colouring mattersemployed are the…
Textile printing