G silky feeling to the goods. One or two runs are sufficient for thispurpose if the goods have been singed; if unsinged, more runsmust be given. The cloth is then ready for the shear. Shearing. This class of worsteds is closely sheared, butshould not be scraped. On the rubber rest shear several… … Fig. 79. Kinyon Bros. Dampening Machine. are also steamed and rolled upon the press. This process will dofor light-weights or simple fabrics. The heavier goods, or those having a wool back, are alsosinged, but fulling takes the place of crabbing. They are run ina fulling mill for fifteen or twenty…
Woolen and worsted manufacture · Textile finishing
Internet Archive · Library of Congress · Public Domain Mark 1.0. Free to use for anything.